SQ Cutters

         Common Solutions to Bad Dressings


Phone: 330-487-0600

1780 Enterprise Parkway 

​twinsburg, Ohio  44087 

    Semtorq, Inc.        
       Serving the industry since 1957 with process Automation and Engineering

Our special design cutters will provide you solutions to your dressing problems

     -Optimized cutter designs enable consistent removal

     -Cutters utilize a four blade configuration for balanced                    dressing

     -Semtorq's SQ cutters maximizes cap life


Problem: Electrode is cut but not cleaned at the weld face after first dress

Probable Cause:  -Too high of weld count before first dress

                                 -Too low of dress force

                                 -Not enough dwell time

                                 -check water flow

                                 -Excess heat accelerates mushrooming